There are two main methods for manufacturing PCBN blades: one is a one-time polymerization, that is, directly using hexagonal boron nitride (HBN) to polymerize into a high-density sintered body. The other is a secondary polymerization method. This method first synthesizes high-density cubic boron nitride (CBN), and then uses high temperature and high pressure as a raw material to form polycrystalline cubic boron nitride. At present, secondary polymerization methods with added binders are more common:


Come fare PCBN Blades??

1. Aggiungere legante metallico CBN sinterizzazione

Ci sono molti tipi di leganti metallici, principalmente Ni, Co, Ti, ti - al, ecc Alla temperatura di sinterizzazione, il legante metallico diventa la fase liquida. La comparsa della fase liquida ha un certo effetto di promozione sulla sinterizzazione CBN, e la sinterizzazione può essere effettuata ad una temperatura e pressione leggermente più basse. Inoltre, poiché il CBN è insolubile nel legante metallico, il processo di dissoluzione e precipitazione che può promuovere il restringimento e la crescita del cristallo non si verificherà. Durante il processo di sinterizzazione, il cobalto nel carburo cementato penetra nel contorno di grana CBN allo stato liquido, e il carburo cementato è strettamente legato al corpo sinterizzato CBN. La durezza dello strumento PCBN con un legante metallico è inferiore a quella dello strumento sinterizzato CBN puro, ma la sua durezza è buona. Marchi come Element Six AMB90, GE BZN6000 e Mitsubishi MB710 sono tutti realizzati nel legante metallico sinterizzato.

2. L'aggiunta di legante in ceramica CBN sinterizzazione

Ceramic binder mainly includes TiN, TiC, Al2O3, etc. Crack due to sintering process, so much in the vitrified bond of iron group elements (iron, cobalt, nickel) and Mo or Mo2C increase strength between ceramic ion, have the effect of the medium of fluid transmitting pressure, is conducive to form internal sintered body without deformation, such as molybdenum can also improve the wettability between ceramic particles and iron. Ceramic binder PCBN binder content is generally higher, toughness than metal binder tool is poor, but its high-temperature resistance performance is better. Such products include DBA80 and DBC50 of British Element six company, BZN7000S and BZN8200 of American GE company, and NBX300 and NBX3200 of Sumitomo Japan.

3. Pure sinterizzazione CBN

Il nitruro di boro cubico policristallino può anche essere formato da un metodo di sinterizzazione diretto in modo che un legante non sia utilizzato nel policristallo CBN. La ricristallizzazione e la crescita del grano si verificano durante la sinterizzazione CBN. I granelli del policristallino CBN dopo la sinterizzazione non sono le particelle di cristallo CBN singole originali. Questo tipo di strumento PCBN ha una buona resistenza all'usura e una lunga durata, ma è difficile rendere la lama con elevata tenacità e grandi dimensioni a causa della sua fragilità e condizioni di temperatura difficili.

La rettificatrice Demina utensile può macinare le lame PCBN ad alta efficienza. Può macinare il bordo e l'arco circolare delle lame PCBN.

Ulteriori informazioni sui nostri prodotti Per saperne di più